This method measures the force perpendicular to the plane of the paper required to tear multiple pliesthrough a specified distance after the tear has been started using an Elmendorf-type tearing tester. It does not measure edge-tear resistance. The measured results may be used to calculate the approximate tearing resistance of a single sheet. It is not suitable for single-ply tear testing.

For highly directional boards and papers, prepare specimens according to T 496 Specimen Preparationfor Cross Directional Internal Tearing Resistance for Paper, Paperboard and Related Materials.

Caution is recommended in interpreting results from weakly bonded sheets, especially those containinglightly refined long-fibered chemical pulps. The low rate of tear when multiple plies are torn simultaneously may produce erroneously high results.

Product Details

Published:
11/01/2012
Number of Pages:
6
File Size:
1 file , 74 KB

You may also like

TAPPI T275 sp-23

TAPPI T275 sp-23

Screening of pulp (Somerville-type equipment)standard by Technical Association of the Pulp and Paper Industry, 06/01/2023

TAPPI TIP 0402-32

TAPPI TIP 0402-32

Guidelines for Thermal Spray Coatings Installed to Prevent Corrosion in Pulp Mill Process Equipmentstandard by Technical Association of the Pulp...

TAPPI T271 om-23

TAPPI T271 om-23

Fiber Lenth of Pulp and Paper by Automated Optical Analyzer Using Polarized Lightstandard by Technical Association of the Pulp and...

TAPPI T 551 om-23

TAPPI T 551 om-23

Thickness of Paper and Paperboard (Soft Platen Method)standard by Technical Association of the Pulp and Paper Industry, 06/01/2023

Back to Top