AASHTO TP 127-17 (2019)

AASHTO TP 127-17 (2019)

Click here to purchase
AASHTO TP 127-17 test method covers the determination of fracture energy density of asphalt binder by means ofa direct tension test. For evaluation of relative cracking performance, it is recommended that thistest procedure be used with asphalt binder aged using T 240 (RTFO) plus R 28 (PAV). However,this test can be used for determination of binder facture energy for any binder including any aged(RTFO plus PAV or PAV only) neat or modified binder and asphalt binder extracted andrecovered from pavement. The test apparatus is designed for testing within the intermediatetemperature range, from 0°C to 25°C.

Product Details

Published:
2018
Number of Pages:
25
File Size:
1 file , 2.3 MB

You may also like

AASHTO M 322M/M 322-22

AASHTO M 322M/M 322-22

Standard Specification for Rail-Steel and Axle-Steel Deformed Bars for Concrete Reinforcement (ASTM Designation: A996/A996M-16)standard by American Association of State and...

AASHTO PP 94-22

AASHTO PP 94-22

Standard Practice for Determination of Optimum Asphalt Content of Cold Recycled Mixture with Foamed Asphaltstandard by American Association of State...

AASHTO M 235M/M 235-22

AASHTO M 235M/M 235-22

Standard Specification for Epoxy Resin Adhesives (ASTM Designation: C881/C881M-20a)standard by American Association of State and Highway Transportation Officials, 2022

AASHTO R 70M/R 70-22

AASHTO R 70M/R 70-22

Standard Practice for Use of Apparatus for the Determination of Length Change of Hardened Cement Paste, Mortar, and Concrete (ASTM...

Back to Top