This test method covers the determination of an asphalt binder’s resistance to ductile failure using a double-edge-notched tension (DENT) test.

The test is conducted after thermal conditioning to determine the essential work of failure, the plastic work of failure, and an approximate critical crack tip opening displacement at a specified temperature and rate of loading.

Product Details

Published:
2022
Number of Pages:
11
File Size:
1 file , 550 KB
Note:
This product is unavailable in Ukraine, Russia, Belarus

You may also like

AASHTO M 322M/M 322-22

AASHTO M 322M/M 322-22

Standard Specification for Rail-Steel and Axle-Steel Deformed Bars for Concrete Reinforcement (ASTM Designation: A996/A996M-16)standard by American Association of State and...

AASHTO PP 94-22

AASHTO PP 94-22

Standard Practice for Determination of Optimum Asphalt Content of Cold Recycled Mixture with Foamed Asphaltstandard by American Association of State...

AASHTO M 235M/M 235-22

AASHTO M 235M/M 235-22

Standard Specification for Epoxy Resin Adhesives (ASTM Designation: C881/C881M-20a)standard by American Association of State and Highway Transportation Officials, 2022

AASHTO R 70M/R 70-22

AASHTO R 70M/R 70-22

Standard Practice for Use of Apparatus for the Determination of Length Change of Hardened Cement Paste, Mortar, and Concrete (ASTM...

Back to Top